Precision Brush Plating Restores Connector Pin Conductivity

2026-11-26
Latest company news about Precision Brush Plating Restores Connector Pin Conductivity

Brush plating has become a targeted method for repairing worn connector pins in avionics, precision electronics and field maintenance, where conventional tank plating can be costly and time-consuming. By confining the electrolyte to a pen tip, the process deposits metal only at the contact point and allows repairs to be performed in place. The technique depends on a nickel underlayer and controlled voltage settings to restore conductivity and corrosion resistance.

In-place repair versus tank plating

In avionics maintenance and precision electronics rework, worn plating on connector pins can reduce electrical performance. Traditional tank plating requires the entire component to be removed and masked, a process that extends turnaround time and increases cost. Brush plating is designed to address the same wear issue by depositing metal only where the pen tip makes contact, enabling localized repair without full disassembly.

Why a nickel barrier is required

Gold offers strong corrosion resistance and conductivity, but it cannot be plated directly onto a copper substrate. When wear exposes the copper base, a nickel layer must first be deposited. The nickel layer bonds well to copper and acts as a diffusion barrier that prevents copper atoms from migrating into the gold layer, helping maintain contact stability over time.

For non-copper substrates such as brass or steel, a copper flash step is required before nickel deposition to provide a compatible transition layer.

Standard operating procedure

The repair sequence combines surface preparation, controlled deposition and a final cleaning step. Voltage settings vary by stage, with the workpiece connected to the negative terminal and the plating pen connected to the positive terminal.

  1. Surface cleaning: Remove oxidation with a metal polish and wipe the area with a lint-free cloth.
  2. Degreasing: Use a degreasing pen (PL-1002) at 10–12 V. Move the pen gently until small bubbles appear. Stainless steel requires a dedicated degreasing pen (PL-1014).
  3. Copper flash (non-copper substrates only): Apply a thin copper layer with a copper pen (PL-1010) at 6–8 V.
  4. Nickel underlayer deposition: Deposit nickel with a nickel pen (PL-1006) at 5–6 V to form the diffusion barrier.
  5. Gold layer deposition: Switch to a 24K gold pen (PL-1003) and apply evenly at 6–8 V until the desired thickness is reached.
  6. Finishing: Rinse with clean water and dry with a soft cloth.
Deposition performance

Deposition rates vary by pen type and application time. The table below summarizes typical thickness figures for standard and heavy gold and nickel pens.

Pen type 2-minute deposition thickness 3-minute deposition thickness Maximum thickness
Gold 24K (PL-1003) 0.5 µm 0.8 µm 1.5–1.8 µm
Gold 24K Heavy (PL-1016) 0.8 µm 1.2 µm 3–3.6 µm
Nickel (PL-1006) 0.4 µm 0.6 µm 1.5–1.8 µm
Nickel Heavy (PL-1020) 0.8 µm 1.2 µm 3–3.6 µm
Frequently Asked Questions
Can gold be plated directly onto copper pins?
No. Gold cannot adhere directly to a copper substrate. A nickel layer must first be deposited as a diffusion barrier to prevent copper migration and protect conductivity.
Must a connector be disassembled for pin repair?
Usually not. Because brush plating deposits metal only at the point where the pen tip contacts the surface, localized repair can be performed while the connector remains installed, without full tank plating.
What voltage settings are used during plating?
Degreasing uses 10–12 V DC, nickel underlayer deposition uses 5–6 V, and gold deposition uses 6–8 V. The workpiece is connected to the negative terminal and the plating pen to the positive terminal.